Japan SMC cylinder bore size represents the size of the cylinder output force. Piston in the cylinder to make a smooth reciprocating sliding, the surface roughness of the surface of the cylinder barrel should reach Ra0.8um. Of the steel cylinder, the inner surface should be hard chromium plated to reduce friction and wear, and to prevent corrosion. In addition to cylinder material carbon steel tubing or high-strength aluminum alloy and brass. Stainless steel cylinder with a small tube. Cylinder with a magnetic switch or corrosion environment in the cylinder, the cylinder should use stainless steel, aluminum or brass and other materials.
Japanese SMC cylinder piston is under pressure in the parts. About two-chamber piston to prevent gas channeling each other, with the piston ring. Wear on the piston ring can improve the orientation of the cylinder, the piston ring to reduce wear, reduce friction. Long use of polyurethane wear ring, PTFE, synthetic resin, cloth and other materials. The width of the size of the piston ring and necessary to determine the length of the sliding part. Sliding part of the short, easy to cause early wear and tear and stuck. Material commonly used aluminum pistons and cast iron, a small cylinder made ​​of brass piston.
  Japanese SMC air cylinder piston rod is the most important force components. Typically use high-carbon steel, hard chrome plated surface, or use stainless steel to prevent corrosion and increase the wear resistance of seals.

版权与免责声明

1、凡本网注明"来源:亚洲建材网"的所有作品,版权均属于亚洲建材网,转载请必须注明亚洲建材网,https://www.a-bm.cn/。违反者本网将追究相关法律责任。

2、企业发布的公司新闻、技术文章、资料下载等内容,如涉及侵权、违规遭投诉的,一律由发布企业自行承担责任,本网有权删除内容并追溯责任。

3、本网转载并注明自其它来源的作品,目的在于传递更多信息,并不代表本网赞同其观点或证实其内容的真实性,不承担此类作品侵权行为的直接责任及连带责任。其他媒体、网站或个人从本网转载时,必须保留本网注明的作品来源,并自负版权等法律责任。

4、如涉及作品内容、版权等问题,请在作品发表之日起一周内与本网联系,否则视为放弃相关权利。

QQ联系

咨询中心
客服帮您轻松解决~

联系电话

参展咨询0571-8894 7171会议咨询0571-8894 7171

建议反馈

返回顶部